Forming quality,mechanical properties,and anti-inflammatory activity of additive manufactured Zn–Nd alloy
增材制造制备Zn–Nd合金的成形质量、力学性能及抗炎活性作者机构:Institute of Biadditive ManufacturingJiangxi University of Science and TechnologyNanchang 330013China State Key Laboratory of High Performance Complex ManufacturingCentral South UniversityChangsha 410083China Shenzhen Institute of Information TechnologyShenzhen 518172China Jiangsu Key Laboratory of Precision and Micro-Manufacturing TechnologyNanjing University of Aeroncautics and AstronauticsNanjing 210016China School of Basic Medical ScienceCentral South UniversityChangsha 410083China School of Energy and Machinery EngineeringJiangxi University of Science and TechnologyNanchang 330013China
出 版 物:《Journal of Zhejiang University-Science A(Applied Physics & Engineering)》 (浙江大学学报(英文版)A辑(应用物理与工程))
年 卷 期:2020年第21卷第11期
页 面:876-891页
核心收录:
学科分类:08[工学] 080502[工学-材料学] 0805[工学-材料科学与工程(可授工学、理学学位)] 0802[工学-机械工程] 080201[工学-机械制造及其自动化]
基 金:the National Natural Science Foundation of China(Nos.51935014,82072084,and 81871498) the Jiangxi Provincial Natural Science Foundation of China(Nos.20192ACB20005 and 2020ACB214004) the Jiangxi Provincial Key R&D Program(No.20201BBE51012) the Guangdong Provincial Higher Vocational Colleges&Schools Pearl River Scholar Funded Scheme(2018) the China Postdoctoral Science Foundation(No.2020M682114) the Open Research Fund of Jiangsu Key Laboratory of Precision and Micro-Manufacturing Technology the Project of Hunan Provincial Science and Technology Plan(No.2017RS3008),China
主 题:Zn–Nd alloy Laser powder bed fusion(LPBF) Anti-inflammatory activity Mechanical properties
摘 要:Zinc(Zn)has recently been recognized as a promising bone repair material due to its inherent biodegradability and favorable *** this work,rare earth neodymium(Nd)was introduced into a Zn-based alloy fabricated using a laser powder bed fusion(LPBF)*** showed that addition of Nd significantly improved the melt fluidity and reduced the evaporation of Zn,thereby achieving parts with a high densification rate of 98.71%.Significantly,the Nd alloying treatment effectively refined the grain size from 25.3 to 6.2μ*** Zn5 eutectics precipitated and contributed to a second-phase strengthening *** a result,the tensile strength increased to(119.3±5.1)MPa and the Vickers hardness to(76.2±4.1).Moreover,the Zn–Nd alloy exhibited good anti-inflammatory activity,as the Nd ions released during degradation had a strong affinity with cell membrane phospholipids and consequently inhibited the release of inflammatory *** also presented favorable cytocompatibility,showing great potential as a bone repair material.