Active Air Venting of Mold Cavity to Improve Performance of Injection Molded Direct Joining

作     者:Fuminobu Kimura Shotaro Kadoya Yusuke Kajihara Fuminobu Kimura;Shotaro Kadoya;Yusuke Kajihara

作者机构:Institute of Industrial ScienceThe University of Tokyo4-6-1KomabaMeguro-kuTokyoJapan 

出 版 物:《Nanomanufacturing and Metrology》 (纳米制造与计量(英文))

年 卷 期:2021年第4卷第2期

页      面:109-117页

核心收录:

学科分类:0817[工学-化学工程与技术] 08[工学] 0807[工学-动力工程及工程热物理] 0805[工学-材料科学与工程(可授工学、理学学位)] 080502[工学-材料学] 0802[工学-机械工程] 0811[工学-控制科学与工程] 0801[工学-力学(可授工学、理学学位)] 

基  金:This study was supported by JSPS KAKENHI(#17J00345)and the Foundation for the Promotion of Industrial Science.A part of the experiments was carried out with the supports and advices of Yokoi group the University of Tokyo Japan 

主  题:Metal-plastic direct joining Micro-/nano-structured surface Injection molding Active venting Mold cavity pressure measurement 

摘      要:A surface micro-/nano-structured metal plate can be joined with an injection molded plastic piece in a mold,which has been named injection molded direct joining(IMDJ).The injected plastic melt infiltrates the micro-/nano-structure,e.g.,a porous structure with micro/nano pores,on the metal plate while flowing in the mold cavity where the metal plate is *** solidification of the plastic,the metal and plastic materials are directly joined via the micro-/nano-structured metal *** air is trapped by the plastic melt,it is easily imagined that the air in the mold cavity prevents the melt plastic from contacting the metal surface and infiltrating the micro-/nano-structure,which could result in poorer joining *** avoid the prevention of the air for the better joining performance,the present study proposes a system actively venting the mold cavity during injection *** apply the active venting to IMDJ,venting and sealing systems were newly *** addition,a system measuring air pressure of the mold cavity was *** proposed system was evaluated by a measurement of joining strengths of IMDJ specimens that were produced under various *** the results,it is concluded that the active venting does not necessarily have a positive effect in any cases:the effect depends on the type of surface micro-/nano-structure.