PROPERTIES OF (***) BO_3: Eu^(3+)PHOSPHORS SYNTHESIZED BY MICROWAVE HEATING METHOD
PROPERTIES OF (Y. Gd) BO_3: Eu ̄(3+)PHOSPHORS SYNTHESIZED BY MICROWAVE HEATING METHOD作者机构:Department of Chemistry Zhongshan University Guangzhou 510275 Department of Chemistry Juin University Changchun 130023
出 版 物:《Chinese Chemical Letters》 (中国化学快报(英文版))
年 卷 期:1996年第7卷第4期
页 面:387-388页
核心收录:
学科分类:081704[工学-应用化学] 07[理学] 08[工学] 0817[工学-化学工程与技术] 0703[理学-化学] 070301[理学-无机化学]
主 题:Gd OF PROPERTIES HEATING MICROWAVE METHOD PHOSPHORS SYNTHESIZED Eu BO3
摘 要:In this peper we have synthesized powder crystal form (Y,Gd) BO3:Eu(3+)Phosphors by microwave heating method. ItS structure belongs to hexagonal system with lattice parameters a=0.3796,c=0. 8835. Its excitation spetra peaks at 239.0nm and 240. 0nm monitored at the emission of 589nm and 612nm respectively, the half peak width is 40nm. Under 240nm excitation the phosphors show a strons oranse-red luminescence, the fluorescent intensity ratio for I589/I612 is 1.9/1