Corrosion behavior of pure aluminum in FeCl_3 solution
Corrosion behavior of pure aluminum in FeCl_3 solution作者机构:School of Chemistry and Material ScienceHubei University Department of ChemistryHuazhong University of Science and Technology Postdoctoral Station of Technical Institute of Physics and ChemistryChinese Academy of Sciences
出 版 物:《Transactions of Nonferrous Metals Society of China》 (中国有色金属学报(英文版))
年 卷 期:2006年第7卷第6期
页 面:1460-1466页
核心收录:
学科分类:080503[工学-材料加工工程] 0806[工学-冶金工程] 08[工学] 0805[工学-材料科学与工程(可授工学、理学学位)]
主 题:pure aluminum pitting corrosion FeCl3 solution AFM uniform attack
摘 要:The corrosion behavior of pure aluminum in FeCl3 solution was investigated mainly by in-situ AFM(Atomic Force Microscopy).The results of combined researches of AFM,SEM(Scanning Electron Microscopy)and EDAX(Energy Dispersive Analysis of X-ray)show that in addition to uniform attack,pitting corrosion takes place also on pure aluminum surface in FeCl3 solution at open-circuit potential,and impurity elements Fe and Cu are found enriched in corrosion ***-situ AFM was also used to examine the initiation and development of pitting corrosion of pure aluminum induced by potentiodynamic sweep,and the repassivation of an active pit is *** tip scratching technique was used to produce a physical defect on metal surface,which is traced by in-situ AFM and it is found that the defect is likely to be preferentially attacked and evolve to pitting corrosion.