Reaction behaviors of Pb and Zn sulfates during reduction roasting of Zn leaching residue and flotation of artificial sulfide minerals
Reaction behaviors of Pb and Zn sulfates during reduction roasting of Zn leaching residue and flotation of artificial sulfide minerals作者机构:State Key Laboratory of Complex Nonferrous Metal Resources Clean UtilizationKunming University of Science and TechnologyKunming 650093China Faculty of Land Resource EngineeringKunming University of Science and TechnologyKunming 650093China School of Minerals Processing and BioengineeringCentral South UniversityChangsha 410083China
出 版 物:《International Journal of Minerals,Metallurgy and Materials》 (矿物冶金与材料学报(英文版))
年 卷 期:2021年第28卷第3期
页 面:358-366页
核心收录:
学科分类:0709[理学-地质学] 0819[工学-矿业工程] 081902[工学-矿物加工工程] 0806[工学-冶金工程] 08[工学] 0708[理学-地球物理学] 0805[工学-材料科学与工程(可授工学、理学学位)] 0703[理学-化学] 0802[工学-机械工程] 0702[理学-物理学] 0801[工学-力学(可授工学、理学学位)]
基 金:the National Natural Science Foundation of China(No.51964027) the Yunnan Province Applied Basic Research Project,China(No.2017FB084) the Foundation of Yunnan’s Education Ministry,China(No.2019J0037) the Testing and Analyzing Funds of Kunming University of Science and Technology(No.2018T20150055)
主 题:zinc leaching residue reduction roasting flotation Pb and Zn sulfates artificial sulfides
摘 要:To evaluate the feasibility of recovering Pb and Zn sulfides and Ag-containing minerals from Zn leaching residue by the process of reduction roasting followed by flotation,the reaction behaviors of Pb and Zn sulfates during this process were *** analysis showed that the transformation ratios of PbSO4 and ZnSO4 could reach 65.51%and 52.12%,respectively,after reduction roasting,and the introduction of a sulfidation agent could improve the transformation ratios of these *** electron microscopy-energy dispersive spectroscopy(SEM-EDS)revealed that temperature obviously affects the particle size,crystal growth,and morphology of the artificial Pb and Zn sulfide *** size analysis demonstrated that the particle size of the materials increases after *** tests revealed that a flotation concentrate composed of 12.01wt%Pb,27.78wt%Zn,and 6.975×10^(−2)wt%Ag with recoveries of 60.54%,29.24%,and 57.64%,respectively,could be obtained after roasting.